MMS- Are some unreliable with high RH?

#61
Whats a non-approved special adhesive mean? I've never heard that before, jeez
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#62
Unapproved. He sold the customer on magic glue that isn't magic at all.
Reply

#63
(11-16-2011, 06:52 PM)eaadams Wrote:  Unapproved. He sold the customer on magic glue that isn't magic at all.

Uapproved for what flooring and by whom? Can't you be more specific, I ain't no mind reader here.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#64
We as the manufacture only allow three different adhesives. This guy bought his own and he is now on his own.
Reply

#65
(11-16-2011, 07:26 PM)eaadams Wrote:  We as the manufacture only allow three different adhesives. This guy bought his own and he is now on his own.

There's my point right there.

Manufacturers will quickly wash their hands of jobs that don't follow their requirements or use unapproved materials. And they have the right to! They know what they need to have to perform as designed.

JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,306 08-20-2012, 07:07 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,078 12-08-2011, 06:03 PM
Last Post: Ernesto
  high rh in concrete chas04344 2 8,907 09-11-2009, 07:33 PM
Last Post: chas04344

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)