High Rapid RH readings??

#21
Bottom line, you have a wet slab.

RH levels do actually fall rather quickly once the slab starts drying. By rather quickly I mean a 1 - 2 points a week if conditions are right.

As long as you have done the testing according to the instructions in your test kit, you can trust the readings. You should be 2.4" into the slab, brushed and vacuumed holes, drilled straight and true, you don't wet drill right?

If it makes you feel any better, I did a job last fall where they waited 16 months for suspended floors to dry and they were still at 98%. The 4" slab on grade areas were down to the mid 80's to low 90's.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#22
6" slab, 3 months for the first 4" and 2 months more for 2" more. I have a 5" slab in Sacramento made the same way. It sat at 99% for four months then dropped to 91% then dropped to 88% the next month. Have patience. When in doubt, blame the structural engineer who build a 6" slab for a small room. They SE's are the source of >90% of my issues.
Reply

#23
Once back in the early 80's I went to do some vinly out in the sticks. Some dude out there was building custom ranch houses. As I was driving into the development...these were like 20 acre parcels each. I drove by a newly poured slab which had sprinklers spraying water on it.

When I asked WTF with the sprinklers, he started into this thing about how it hardens the concrete and keeps it from cracking. The sprinklers had been wetting the slab for a month.

Got into the house and the concrete was black with white-ish patches all over it. What did I do next?
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#24
I just did a floor in a gym done with sprinklers. It turned out great and the RH got down into the 80's in a fair amount of time.
Reply

#25
Wet curing is the way we recommend all concrete be cured that is going to receive moisture sensitive flooring. I recommend a 3 day wet cure.
The longer concrete is kept wet, the harder it gets.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#26
I like to see burlap over the top myself. That guy was sprinkling the surface and it was pitted.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#27
Burlap is put down to hold the moisture. They wet the burlap. Water can't be put on the concrete until it is hard enough to resist damage.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#28
(11-12-2011, 05:13 PM)CC Solutions Wrote:  Burlap is put down to hold the moisture. They wet the burlap. Water can't be put on the concrete until it is hard enough to resist damage.

Yea well you go tell that to that old rancher dude. I bet he will run you off his property with a shotgun
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#29
ok so,

the independent lab of my client will be retesting the floor with their nucleo meter and the flooring contractor will be testing it with his meter this week. I predict both meters will read that the floor is ready (or near-ready since 2 weeks ago, only 1 percentage point lower was needed to start). But ofcourse that's at the surface.

My Rapid RH are reading below surface which is the right reading, BUT everyone is having trouble trusting this "new" technology, especially when the readings haven't moved.

So here is my dilemma, do i let them go ahead and do the floor or do i be an "a-hole" and tell them to its not ready? Maybe they should do it. After all they are responsible should something happen and the flooring contractor has to guarantee the floor. Right? But should the floor fail, it will be huge head-aches for me since I am the GC.

Q1: Does anyone know what the Rapid RH reading has to be at for my type of installation ("floating" type)? From my research, I've read it has to be at about 80%.

Q2: Has anyone installed wood floor at high RH (and how high) and didn't have problems?

Thanks.

Reply

#30
(11-16-2011, 10:05 AM)ddemento Wrote:  So here is my dilemma, do i let them go ahead and do the floor or do i be an "a-hole" and tell them to its not ready? Maybe they should do it. After all they are responsible should something happen and the flooring contractor has to guarantee the floor. Right? But should the floor fail, it will be huge head-aches for me since I am the GC.

This is the problem I have with GC's. If the floor is reading high it is reading high. You have a duty to your customer to build a building that will not have problems. Don't do it. Don't risk it. If you get sued how much will the legal bills cost you? More than doing it right the first time.

For Q1 you need to contact the manufacturer. Go around your sub if he isn't competent enough to understand RH. Every reputable manufacturer knows RH. Every reputable manufacturer has a local rep who should know rh.

For Q2 this is a bad question. Asking if anyone has installed a wood floor over high RH is like asking has anyone painted a wall. There are thousands of different paints for walls.

If your RH is high, don't do it. Go get your own expert.
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Who Says Rapid Rh Reads High? Ernesto 3 9,340 08-20-2012, 07:07 PM
Last Post: CC Solutions
  Ardex promotes the Wagner Rapid RH probe! CC Solutions 15 35,196 01-15-2012, 06:33 PM
Last Post: CC Solutions
  MMS- Are some unreliable with high RH? Rubensgt40 64 102,260 11-17-2011, 07:56 AM
Last Post: CC Solutions
  No Love - August Rapid RH Newsletter eaadams 4 9,376 08-19-2011, 07:13 AM
Last Post: CC Solutions
  A GC wants a second opinion, and the first readings were Wagner's! CC Solutions 2 6,824 08-14-2011, 07:56 PM
Last Post: Ernesto
  Multiple Readings? GregR 6 13,729 11-19-2010, 05:26 PM
Last Post: CC Solutions
  high rh in concrete chas04344 2 8,934 09-11-2009, 07:33 PM
Last Post: chas04344
  Rh readings dennismck 1 7,946 10-15-2008, 11:00 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)