Last time I was there...2008 I was attending an inspectors seminar and stayed at the Flamingo Las Vegas. The bed was so lopsided I kept rolling off it, so I just went downstairs and stayed up the rest of the night.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#12
You have 2 year old concrete that is at 90% RH?
(10-21-2011, 07:26 PM)Ernesto Wrote:  Last time I was there...2008 I was attending an inspectors seminar and stayed at the Flamingo Las Vegas. The bed was so lopsided I kept rolling off it, so I just went downstairs and stayed up the rest of the night.

Yeah.... "Honey the bed was so bad I kept rolling off so I figured I may as well gamble and drink all night.... "

Did that story fly for you?? LOL Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#13
It was a series of articles in concrete construction magazine called the long term field test.

In the final review after two years the rh of the slab poured inside with a roof on still had rh unacceptably high.

Still waiting on some further examination from the magazine. However the space was probably leased preventing further investigation of the concrete by the magazine and associated companies.

Wagner was a sponsor of the test and the first set of results were given at a breakfast at Woc 2009.

Reply

#14
I am familiar with the test. The slab was sealed! That was the whole point of the study wasn't it? It showed how mechanically sealing the concrete can retain moisture.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Wagner Playlist eaadams 2 4,460 05-10-2013, 10:17 AM
Last Post: CC Solutions
  Wagner hoodie? Rubensgt40 19 23,172 08-24-2012, 08:39 PM
Last Post: Ernesto
  Wagner Article Vapor Retarders eaadams 2 5,776 06-19-2012, 01:52 PM
Last Post: CC Solutions
  Is Wagner seeking volunteers to help out in Germany at Domotex? CC Solutions 11 21,812 11-17-2011, 04:54 PM
Last Post: Ernesto

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)