Walgreen's Slabs

#1
Anyone know what the thickness of a Walgreen's slab is? I'm assuming they are all built alike, but then thats assuming. Theres no way I am drilling all the way through this baby. The vct has glue seeping through the seams.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#2
We used to do a lot of Sports Authorities and a lot of Rite Aids.

You can never be sure. It is an issue I always have. I usually assume 4" slabs UON. And specify that is the assumed thickness Unless Otherwise Noted.

Put it back on the owner of the building (usually not walgreen's) to dig into records.
Reply

#3
Yea, maybe I should drill all the way through then...sigh. I'm only dealing with a store manager, and a flooring/janitorial service. I doubt either one knows.

I better bring along some corks in case I hit water.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#4
I'd just drill it. A 1/2 inch hole is all you need, then stick a wire with a hook on the end in the hole and feel for the bottom. The antenna from a '68 Barracuda works the best.

You can fill the hole with two part epoxy, or to save money crumple up a couple of $20 bills to stuff in the bottom of the hole then use epoxy. Drill the hole in an out of the way place so if it ever morphs into a geyser you won't have a problem on your hands.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#5
Hmmmm, Thats going to be noisy and more time consuming. You guys ever do them in stores that are open? I'm thinking I better do it before it opens. But man thats pretty early for me. ZZZZZZZZZ
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#6
I did it in a jail recently. Heh try getting a diamond drill bit and utility knife through jail security. Fun.
Reply

#7
You can be through that slab in under a minute... I've done it in hospitals above operating rooms. I figure by the time they can get the maintenance guy alerted and he can find me, I'm long gone.... Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#8
Maybe I'll just drill it for a normal 4 inch slab since the floorcovering is already in place and the rh has already equillibrated, eh? I should get a decent reading in a couple days.Confused
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#9
If you do 4" and it comes in high you know the only way it is a false 'high' test is if the slab is less than 4". Per Jason's post re: what will give a false positive. (a hole drilled too deep was one example, along with aggregate etc..)
Reply

#10
Yes, there's no way a commercial slab is less than 4" in depth.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  How about heated slabs? CC Solutions 4 5,527 12-20-2013, 10:23 PM
Last Post: CC Solutions
  RH Testing Thick Slabs CCR 33 48,001 11-21-2012, 10:19 AM
Last Post: eaadams
  Many are surprised to find OLD slabs are VERY WET! CC Solutions 6 16,047 12-22-2010, 07:37 PM
Last Post: Ernesto

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)