I know the requirement is 40% of slab thickness.
We are getting some very high RH readings (20% higher than the tramex readings) using these probes.
Would RH readings increase as the volume of the space beneath the reader increases?
I am not sure if the technician seated the probes properly (all the way on the bottom of the hole) and if he didn't, can i just push them all the way down and receive accurate readings?
Thanks
Reply

#2
(02-06-2009, 10:44 AM)Jphillips Wrote:  I know the requirement is 40% of slab thickness.
We are getting some very high RH readings (20% higher than the tramex readings) using these probes.
Would RH readings increase as the volume of the space beneath the reader increases?
I am not sure if the technician seated the probes properly (all the way on the bottom of the hole) and if he didn't, can i just push them all the way down and receive accurate readings?
Thanks

Mr. Phillips;
The reason for the difference in the readings can be the fact that the probe is not calibrated or it was not left in the hole long enough to equilibrate. some of the probes can take over an hour to equilibrate.
the other factor is the amouynt of dead air space beneath the sensor or sleeve. Some of the sleeves have a lot of dead air space in them
Respectfully
Rayt
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  improper probe depth Rrozema 10 24,035 03-24-2012, 06:12 AM
Last Post: CC Solutions
  Relative Humidity Probe Depth mwoody 10 22,654 03-24-2011, 07:00 AM
Last Post: CC Solutions
  Probe Placement (Depth) CDougherty 2 8,892 01-15-2010, 09:43 PM
Last Post: CC Solutions
  creating the hole for the sensor SDJeff 1 6,892 11-09-2009, 04:39 PM
Last Post: Ben
  RH Test Hole Callout Ben 3 11,283 11-04-2008, 10:03 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)