It kinda reminded me of SLC hmmmmmm I wonder if I could make my own SLC with that additive? Smile

I read the W/C ratio can run anywhere between .35 and .70. If you use that additive in a bag of readymix or say modified thinset would you use less than .35?



http://en.wikipedia.org/wiki/Self-consolidating_concrete
Uh oh....this I didn't know about measuring water.

http://www.concretecountertopinstitute.com/modules/mytube/singlevideo.php?cid=1&lid=17
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#12
omg that video really makes me long for the Metric system
Reply

#13
(09-30-2011, 04:02 PM)eaadams Wrote:  omg that video really makes me long for the Metric system

LightbulbBig Grin

Yea, multiple that by a 100,000 sf slab ho ho
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#14
Yea, a 1111.111111 s/y slab.

I guess I could use trashcans and a pallet scale.
Reply

#15
Where did you find that video? The guy tries to act all scientific "A gallon of water weighs 8.34 pounds and here we have a pint weighing .9920 pounds when it should weigh 1.0425 pounds..."

Whatever... When you start measuring water for your 1500 yard pours using a plastic paint pail from Home Depot let me know....

And Mr. Scientific didn't give us his altitude or the specific gravity of his water either. Water at 10,000 feet weighs differently than water at sea level. Salt water weighs more than distilled water. What is his water?

And who's to say that his Fisher Price scale is accurate? That thing could be FUBAR.

I guess the idea is if you want to make concrete samples of 12 pound batches, weight them out to the 10,000ths of a pound for the best results.Dodgy
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#16
Now don't be Debbie Downer JD. The reasoning behind that me thinks is not so much for slump as it is for color consistancy. As in colored concrete slabs.
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply

#17
A super plasticizer is a high end water reducing agent. What they do is change the electrical charge of the water molicule so that the repell each other rather than attract each other. In essence it thins out the water like placing alcohol in water.
Regards
Rayt
Reply

#18
Now how about my original post and how scc acts in re moisture testing?
Reply

#19
The moisture testing on SSC concrete is the same as normal concrete. SSC concrete because of the low w/c ratio will dry faster. Once it is placed I don't know how you would tell the difference from normal weight concrete.
Regards
Rayt
Reply

#20
You can probably tell by the lack of plasticizers and the fewer moisture related voids left behind. I mean not by looking at it, but a lab could tell you what you have.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,395 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,301 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,249 11-08-2013, 01:41 PM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,826 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,215 01-30-2013, 04:43 PM
Last Post: eaadams
  World of Concrete 2012 eaadams 0 3,426 03-23-2012, 09:40 AM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,514 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Self-leveling concrete - My bonehead mistake CC Solutions 37 65,519 09-20-2011, 10:07 AM
Last Post: CC Solutions
  Concrete Surface Texture eaadams 12 26,952 06-21-2011, 11:47 AM
Last Post: CC Solutions
  Concrete Moisture Control Systems BuilderPDX 8 16,820 06-09-2011, 06:09 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)