Self-leveling concrete - My bonehead mistake

#11
try a barrel of water with blocks of ice to cool the water.
watch the four temperatures; water, powder, ambient and slab. The cooler the better, but not below 50 degrees
Rayt
Reply

#12
I should make a cooling coil to drop in a barrel of ice.... Like I have for cooling beer wort!

I bet 100' of 1/2" copper coiled up with a garden hose fitting on each end and then dropped into a barrel of ice would chill the flowing water just fine.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#13
I know a long coil of tubing in a cooler of ice can keep beer cold for drinking. If you just use blocks of ice you can dip the cooled water out and add more as you need it. Many of the installers using self-levelers in the hot country will use 10 - 15 blockss of ice to chill their water. Try to keep the water temp below 70F. It doesn't have to be as cold, as does beer.
Rayt
Reply

#14
Big Grin Big Grin Big Grin Big Grin
Reply

#15
Wow. Banned. I think that is the first person I saw banned!!
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#16
How does one get banned????? I know there are some that should be!
Rayt
Reply

#17
You mean Admin doesn't give you the 'BAN' button? Wink

JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#18
Normally, when we ban someone for spamming, we delete any junk that they've posted... it looks like we missed that one.

@Ray - If you'd like to be able to ban people, let us know. In the past, we've tried to keep on top of the spammers so you don't have to worry about it.

- admin
Reply

#19
Oooo Oooo !!! Me Me!! Let me ban people!!!

It's part of my plan to take over the internet and then the world!!!! Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#20
(08-28-2011, 02:34 PM)rthompson Wrote:  How does one get banned????? I know there are some that should be!
Rayt

Uh oh JD! Big Grin I think he is talking about you. Tongue

Admin, anytime you give someone or trust somone mod clearence you should give them the button.

Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,399 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,305 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,252 11-08-2013, 01:41 PM
Last Post: eaadams
  Pre Cast / Self Leveling JDJR 6 8,582 05-27-2013, 10:05 AM
Last Post: CC Solutions
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,844 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,216 01-30-2013, 04:43 PM
Last Post: eaadams
  Self consolidating concrete (SCC) eaadams 32 60,288 05-08-2012, 07:04 AM
Last Post: CC Solutions
  World of Concrete 2012 eaadams 0 3,426 03-23-2012, 09:40 AM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,519 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Concrete Surface Texture eaadams 12 26,954 06-21-2011, 11:47 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)