I was called to provide a second opinion on a job not 10 miles from my shop (THAT never happens!).

The original installer used Wagner Rapid RH probes but the readings were too high. Then the GC called me and wanted a second opinion. I talked to him for a while, and talked to the first installer (a good client of mine) and the decision was made. The owners want a second opinion, even if it is with the same testing probes. Wink

So I put in three probes today just to validate the readings that the first installer was getting. I'll go back to check them tomorrow, and then on Sunday afternoon (I have a key ---- Small Town USA!).

My objectives on this job:
Gain and foster trust for the Wagner probes. The GC will use them again.
Teach the GC why the slab isn't drying.
Explain the dangers of flooring on a wet slab.
Offer a user friendly and fast mitigation system to eliminate future problems.

Wish me luck! I've never had a job this close to home!!!!
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#2
The results are in and the probes read exactly the same at 72 hours as they did at 22 hours. They are a bit lower than the first probes that were installed. They are a slight bit deeper in the slab as the installer was told the floor was 4-5 inches thick and I used the 4 inch depth because that's what the blue prints show.
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply

#3
Different spots, different readings even so slight a depth is what I think. Nothing spectacular should happen if the slab is protected.

Quote:My objectives on this job:
Offer a user friendly and fast mitigation system to eliminate future problems.

Isin't that what it's always about?

I had a guy call me for moisture testing on a commercial job last week, just my luck I was in San Diego on a short vacation.Sad
Stephen Perrera dba
Top Floor Installation Co.
http://www.tucsonazflooring.com
http://www.floorsavior.com
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  new wagner product eaadams 6 15,679 03-23-2012, 09:29 AM
Last Post: eaadams
  Ardex promotes the Wagner Rapid RH probe! CC Solutions 15 35,169 01-15-2012, 06:33 PM
Last Post: CC Solutions
  High Rapid RH readings?? ddemento 49 81,194 12-08-2011, 06:03 PM
Last Post: Ernesto
  Product Idea for Wagner eaadams 1 5,932 06-20-2011, 01:53 PM
Last Post: EWagner
  New Wagner Videos from Surfaces 2011 eaadams 11 23,373 04-23-2011, 08:34 PM
Last Post: CC Solutions
  Wagner vs GE Hygromaster, Please Coment mferry4 5 12,413 02-05-2011, 09:36 AM
Last Post: CC Solutions
  Multiple Readings? GregR 6 13,718 11-19-2010, 05:26 PM
Last Post: CC Solutions
  Rh readings dennismck 1 7,937 10-15-2008, 11:00 AM
Last Post: rthompson

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)