What’s the big deal with the HVAC? Do I need it on when testing?
Reply

#2
I think you do, but I'm not quite sure why.
I knew I saw it somewhere. It looks like an project environment issue.

Take a look at the Rapid RH FAQ page. I think that's pretty clear.
Reply

#3
(12-23-2008, 04:15 PM)Chris Reynold Wrote:  What’s the big deal with the HVAC? Do I need it on when testing?

Mr. Reynolds,
It is a good idea, cold conditions will drive the moisture down deeper giving your test results a false positive. Also the HVAC will help get the slab into equalibrium.
Regards
Rayt
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  Moisture going up Rubensgt40 3 1,600 07-05-2014, 03:18 AM
Last Post: Rubensgt40
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,481 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,477 05-19-2014, 10:55 AM
Last Post: eaadams
  Digital moisture meter QC worker 2 1,904 05-10-2014, 08:07 PM
Last Post: Rubensgt40
  Concrete Hood Method Blake McFee 9 27,377 11-08-2013, 01:41 PM
Last Post: eaadams
  Tandus removes moisture testing requirement eaadams 2 4,132 09-27-2013, 10:26 AM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 64,214 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,265 01-30-2013, 04:43 PM
Last Post: eaadams
  Carbide moisture testing CC Solutions 4 8,709 09-18-2012, 06:11 PM
Last Post: CC Solutions
  Self consolidating concrete (SCC) eaadams 32 60,641 05-08-2012, 07:04 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)