Concrete Surface Texture

#11
Ray that is not my point. I'm not looking at removing a surface.

I'm talking about the smoothness needed for resilient sheet flooring. A CSP of 3-4 would need to be re surfaced to put flooring on.
Reply

#12
Concrete should have the texture of about 100 grit sandpaper to obtain a good mechanical bond for sheet vinyl adhesives and especially epoxies. Burnished concrete not only compromises adhesive bond, but retards the moisture drying in a timely fashion. If the moisture is there it is going to get out eventually.
Regards
Rayt
Reply

#13
Agreed Ray. The big issue is open and porous, and sandpaper type texture is an easy reference. Sandpaper is everywhere.

Looking back over the posts, that CC Solutions guy has some good info on this thread... Big Grin
JD Grafton
Concrete Answers for Flooring Problems
[email protected]
Reply


Possibly Related Threads...
Thread Author Replies Views Last Post
  ICRI pH testing Concrete Repair Bulletin eaadams 4 2,353 05-20-2014, 12:00 PM
Last Post: Ashok Kakade
  35-40 year old concrete with moisture problems Tscdad 13 7,175 05-19-2014, 10:55 AM
Last Post: eaadams
  Concrete Hood Method Blake McFee 9 27,172 11-08-2013, 01:41 PM
Last Post: eaadams
  RH in Concrete for Wood Floor with Vapor Membrane eaadams 35 63,584 05-01-2013, 07:20 AM
Last Post: jim decker
Question Concrete Cork Sandwich Floor System JKJeremy 4 8,178 01-30-2013, 04:43 PM
Last Post: eaadams
  Self consolidating concrete (SCC) eaadams 32 59,990 05-08-2012, 07:04 AM
Last Post: CC Solutions
  World of Concrete 2012 eaadams 0 3,416 03-23-2012, 09:40 AM
Last Post: eaadams
  Old concrete slab moisture DeanC 23 50,302 12-15-2011, 01:20 AM
Last Post: foxgeorge
  Self-leveling concrete - My bonehead mistake CC Solutions 37 65,301 09-20-2011, 10:07 AM
Last Post: CC Solutions
  Concrete Moisture Control Systems BuilderPDX 8 16,760 06-09-2011, 06:09 AM
Last Post: CC Solutions

Digg   Delicious   Reddit   Facebook   Twitter   StumbleUpon  


Users browsing this thread:
1 Guest(s)