Wagner Article Vapor Retarders - Printable Version +- Concrete Moisture Measurement Forums (http://www.wagnermeters.com/concreteforum) +-- Forum: Concrete (/forumdisplay.php?fid=1) +--- Forum: General Discussions (/forumdisplay.php?fid=6) +--- Thread: Wagner Article Vapor Retarders (/showthread.php?tid=294) |
Wagner Article Vapor Retarders - eaadams - 06-19-2012 11:29 AM http://www.wagnermeters.com/external-influences-on-concrete-moisture.php?utm_source=iContact&utm_medium=email&utm_campaign=Rapid%20RH%20Newsletter&utm_content=06-12+RRH+Newsletter Check your language. ACI has specific guidelines for the words "Vapor Retarders". I think you are talking more "Vapor Barriers" It is all about the perms and under the slab you want a Barrier at or less than 0.01 perms, stego or equal RE: Wagner Article Vapor Retarders - rapidrhrep - 06-19-2012 12:41 PM You got me. Sloppy language on my part. Jason RE: Wagner Article Vapor Retarders - CC Solutions - 06-19-2012 01:52 PM Way to keep Jason on his toes!!! ![]() Now let's work on that sign off at the end of the videos....
|