coverage - bonedry - 08-22-2009 03:10 PM I am thinking using the RapidRH system but cannot find how many tests should be used for 1000 sqft RE: coverage - jf222 - 08-24-2009 07:36 AM According to the ASTM standard, it's 3 tests for the first 1000 ft^2 and 1 test for each 1000 ft^2 after that. |