RE: Substrate Odor - eaadams - 07-18-2012 11:09 AM

I had a similar project where the Ardex Feather Edge re-emulsified under a ton of ph/water. The whole building is a sick building with 'smell' coming from the floor and the walls and everything.

It turned out that the downspouts for the roof fed down and into the slab, not out through the parking lot. The only way they found that was by hiring a consultant who scoped all the drains.

So if they worry that it is more than the gypsum, perhaps they are making a wise decision to further investigate.


RE: Substrate Odor - CCR - 07-18-2012 11:36 AM

In that sense, I agree. That is if the building maintenance guys are wrong in their belief that all water elimination systems are functioning correctly. Who knows? I suspect I'll learn more in time. Will post any new info I get.