RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011 06:35 PM

Whats a non-approved special adhesive mean? I've never heard that before, jeez


RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011 06:52 PM

Unapproved. He sold the customer on magic glue that isn't magic at all.


RE: MMS- Are some unreliable with high RH? - Ernesto - 11-16-2011 07:12 PM

(11-16-2011 06:52 PM)eaadams Wrote:  Unapproved. He sold the customer on magic glue that isn't magic at all.

Uapproved for what flooring and by whom? Can't you be more specific, I ain't no mind reader here.


RE: MMS- Are some unreliable with high RH? - eaadams - 11-16-2011 07:26 PM

We as the manufacture only allow three different adhesives. This guy bought his own and he is now on his own.


RE: MMS- Are some unreliable with high RH? - CC Solutions - 11-17-2011 07:56 AM

(11-16-2011 07:26 PM)eaadams Wrote:  We as the manufacture only allow three different adhesives. This guy bought his own and he is now on his own.

There's my point right there.

Manufacturers will quickly wash their hands of jobs that don't follow their requirements or use unapproved materials. And they have the right to! They know what they need to have to perform as designed.