Concrete Moisture Measurement Forums
check it out - Printable Version

+- Concrete Moisture Measurement Forums (http://www.wagnermeters.com/concreteforum)
+-- Forum: Concrete (/forumdisplay.php?fid=1)
+--- Forum: Moisture Measurement in Concrete (/forumdisplay.php?fid=2)
+--- Thread: check it out (/showthread.php?tid=217)

Pages: 1 2


check it out - eaadams - 10-27-2011 01:10 AM

www.sportsbuilders.org/events/presentations/pontevedra_4dcraig.pdf

It doesn't make enough of a deal about sand under slabs.

Look at page 111 - now that is a lot of probes.

Look at page 113. What is that?

Look at page 119 - shows how to get a low reading.


RE: check it out - CC Solutions - 10-28-2011 12:05 PM

Wow, how did you get Peter's powerpoint presentation? Huh


RE: check it out - eaadams - 10-30-2011 11:32 AM

I didn't. Google must have indexed the files on that website.


RE: check it out - CC Solutions - 10-31-2011 05:35 AM

Well don't tell him I have it... Big Grin


RE: check it out - Ernesto - 10-31-2011 04:44 PM

Quote:Posted by eaadams - Yesterday 10:32 AM
I didn't. Google must have indexed the files on that website.

Uh huh, thats what they all say when they get caught stealing files.

I posted it all over the internet already, to late.

What goes on the internet, stays on the internet.Rolleyes


RE: check it out - eaadams - 10-31-2011 04:49 PM

Is it stealing if google is the one finding it.

I'm sure the Moderator would have locked this thread if this was improper.


RE: check it out - Ernesto - 10-31-2011 05:49 PM

I was kidding dude, relax. I won't rat you out. Cool


RE: check it out - eaadams - 10-31-2011 06:08 PM

Peter Craig is kinda a big deal. I don't want to upset any Apple carts if you know what I mean.


RE: check it out - Ernesto - 10-31-2011 06:42 PM

(10-31-2011 06:08 PM)eaadams Wrote:  Peter Craig is kinda a big deal. I don't want to upset any Apple carts if you know what I mean.

Yes I know exactly what you mean. However if he is going to be upset about it he should be upset about the website that put it up there without protecting it from being copied or linked, not you. There are ways to do that.


RE: check it out - Rubensgt40 - 10-31-2011 10:34 PM

(10-27-2011 01:10 AM)eaadams Wrote:  www.sportsbuilders.org/events/presentations/pontevedra_4dcraig.pdf

It doesn't make enough of a deal about sand under slabs.

Look at page 111 - now that is a lot of probes.

Look at page 113. What is that?

Look at page 119 - shows how to get a low reading.

111: That's what it looks like when a slab gets acupuncture.
113: Never seen that- I think some adhesives manufacturers use that method, I've heard them referring to something involving PVC tubes.
119: Would that give a low reading? And does ASTM2170 say there shouldn't be clearance between the probe and liner, and no "fins" of any kind?