pH test
|
|
07-08-2010, 10:40 PM
Post: #1
|
|||
|
|||
|
pH test
I notice that wagner sells pH test with distilled water. I thought it was important to use deionized water? As distilled can still carry a charge that can throw off a pH test.
|
|||
|
07-09-2010, 09:33 AM
Post: #2
|
|||
|
|||
|
RE: pH test
From ASTM F710:
5.3.1 To test for pH at the surface of a concrete slab, use wide range pH paper, its associated pH chart, and distilled or deionized water. Place several drops of water on a clean surface of concrete, forming a puddle approximately 1 in. (25 mm) in diameter. From Wagner: Both de-ionization and distillation processes remove ions from the water and produce "pure water". De-ionization processes can leave bacteria in water. Distillation leaves pure water. In terms of quality, distilled water is better. The standard calls for using either. Hope this helps you, eaadams. -admin |
|||
|
07-09-2010, 09:45 AM
Post: #3
|
|||
|
|||
|
RE: pH test
thank you!
|
|||
|