You didn't mention the ambient conditions during the required test period of 72 hours. If the slab is 51 degrees, I would guess the ambient condiitons of the space are not within ASTM F2170-11 standards. The space MUST be placed in operating conditions for 48 hours prior to conductiong the RH test and remain at operating conditions during the 72 hour test period. You need to refer to the document and follow the standards outlined.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
measurement in a cold slab - Noweare - 12-04-2012, 02:45 PM
RE: measurement in a cold slab - CCR - 12-05-2012, 05:47 AM
RE: measurement in a cold slab - CC Solutions - 12-05-2012, 07:37 AM
RE: measurement in a cold slab - Noweare - 12-05-2012, 10:59 AM
RE: measurement in a cold slab - CC Solutions - 12-05-2012, 12:55 PM
RE: measurement in a cold slab - eaadams - 12-19-2012, 01:22 PM
RE: measurement in a cold slab - CCR - 12-19-2012, 02:12 PM
RE: measurement in a cold slab - Ernesto - 12-19-2012, 03:18 PM
RE: measurement in a cold slab - eaadams - 12-19-2012, 03:19 PM
RE: measurement in a cold slab - Ernesto - 12-20-2012, 03:37 PM
RE: measurement in a cold slab - eaadams - 12-20-2012, 04:23 PM
RE: measurement in a cold slab - Ernesto - 12-20-2012, 06:23 PM
RE: measurement in a cold slab - CC Solutions - 12-20-2012, 07:55 PM
RE: measurement in a cold slab - eaadams - 12-21-2012, 04:29 PM
RE: measurement in a cold slab - eaadams - 01-18-2013, 05:02 PM
RE: measurement in a cold slab - eaadams - 11-05-2013, 12:08 PM
RE: measurement in a cold slab - Ernesto - 04-15-2014, 02:30 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 6,901 Views
Last Post by Ernesto
05-05-2014, 04:17 PM
1 Replies 6,364 Views
Last Post by Rubensgt40
01-24-2013, 07:03 PM
23 Replies 66,526 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
2 Replies 12,823 Views
Last Post by CC Solutions
09-20-2010, 02:25 PM
5 Replies 16,259 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 11,383 Views
Last Post by RCConcrete Consulting
09-21-2009, 05:17 PM
1 Replies 11,416 Views
Last Post by EWagner
07-09-2009, 01:46 PM
1 Replies 9,786 Views
Last Post by rthompson
09-26-2008, 02:03 PM

Users browsing this thread:
1 Guest(s)