I do a lot of this type of work in the spring and summer and install a lot of Ardex CD. Was it bad finishing or settling over a poorly prepped sub-base. JD is right, Ardex CD might be just the right product. My advice also is to stay away from ANY exterior self leveler, regardless of the manufacturer or their reputation for self levelers. I've seen too many fixes that don't last.

If it was bad prep before the pour, tear it out and relace it over a well compacted sub-base under a 4" gravel bed!

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
is it possible to replace just two squares of a patio? - lean - 10-11-2012, 11:49 AM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 10-13-2012, 08:39 PM
RE: is it possible to replace just two squares of a patio? - ILLENTINC - 11-15-2012, 02:24 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-15-2012, 02:30 PM
RE: is it possible to replace just two squares of a patio? - ILLENTINC - 11-15-2012, 02:38 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-15-2012, 02:40 PM
RE: is it possible to replace just two squares of a patio? - eaadams - 11-19-2012, 11:26 AM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-19-2012, 09:06 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 06:54 AM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-20-2012, 02:11 PM
RE: is it possible to replace just two squares of a patio? - CCR - 11-20-2012, 02:57 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 03:02 PM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-20-2012, 03:10 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 03:40 PM
RE: is it possible to replace just two squares of a patio? - CCR - 11-20-2012, 03:46 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 05:26 PM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-21-2012, 07:54 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-21-2012, 08:16 PM

Users browsing this thread:
1 Guest(s)