Hello. I just have a concrete patio done. It is cut into rectangles. Two of the rectangles got curvy and rain water stays in them. Can one replace just these two blocks? Is it difficult? Thank you

10-13-2012, 08:39 PM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
Hello and welcome!

Yes you can cut the cupped pieces out and replace them, or you can apply a topical concrete dressing which will fill the low areas, or you could grind them down to be flat (but that will expose aggregate and look kind of weird unless you grind the entire thing.....)

The easiest and fastest would be to apply a concrete repair dressing like Ardex CD. This patch will stand up to vehicle traffic, is easy to mix and place and very fast drying.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

11-15-2012, 02:24 PM #3
ILLENTINC Newbie *
Status: Offline Posts:15 Threads:1 Joined:Aug 2012
(10-11-2012, 11:49 AM)lean Wrote:  Hello. I just have a concrete patio done. It is cut into rectangles. Two of the rectangles got curvy and rain water stays in them. Can one replace just these two blocks? Is it difficult? Thank you

Hello,

If you are still looking for a solution....

Meet MG-Krete by Imco Technologies

http://illianaenterprises.com/meet-mg-krete-by-imco-technologies-2/

MG Krete is the best kept secret and ABSOLUTE BEST option for concrete repair and restoration.

11-15-2012, 02:30 PM #4
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
Let's not turn this forum into a sales platform.... Exclamation

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

11-15-2012, 02:38 PM #5
ILLENTINC Newbie *
Status: Offline Posts:15 Threads:1 Joined:Aug 2012
(11-15-2012, 02:30 PM)CC Solutions Wrote:  Let's not turn this forum into a sales platform.... Exclamation

You recommended a product. I recommended a product.

11-15-2012, 02:40 PM #6
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
I don't sell the product. What you are doing is advertising and it is not allowed here. Sorry.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

11-19-2012, 11:26 AM #7
eaadams Concrete Moisture Expert *****
Status: Offline Posts:597 Threads:86 Joined:Jul 2010
I think CC Solutions should be granted Admin privileges. That is the sort of post that should meet a banhammer.

11-19-2012, 09:06 PM #8
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
That's very ethical of you JD- I know how badly you want to spruke the CC Solutions Concri-Hyper-Mega-Boost 2000*, and the free Packers Cheesy-Head Hat with each purchase.** Big Grin

Grinding is only economical over large areas too. Not many contractors would pull out a grinder for only a couple of square yards or whatnot.

Why would those bits have curled and not others. Are we talking about one pour, cut all the way through, or just feature cuts to the surface?



*fictional product. Don't write in.
**You don't really get a free Green Bay hat. Because it's a fictional product.

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher


11-20-2012, 06:54 AM #9
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
.jpeg images.jpeg Size: 8.62 KB  Downloads: 4


Cheese Head hats fictional? I think not!!!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

11-20-2012, 02:11 PM #10
Rubensgt40 Concrete Moisture Coach ***
Status: Offline Posts:172 Threads:13 Joined:Oct 2011
(11-20-2012, 06:54 AM)CC Solutions Wrote:  Cheese Head hats fictional? I think not!!!

Poor wording on my part- I know the cheesy hats exist, I see them every time I watch NFL replays. Funny how I never have a craving for dry biscuits until I watch a Packers game...

Once again I've driven this post into a ditch Big Grin

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Users browsing this thread:
1 Guest(s)