Yes you can cut the cupped pieces out and replace them, or you can apply a topical concrete dressing which will fill the low areas, or you could grind them down to be flat (but that will expose aggregate and look kind of weird unless you grind the entire thing.....)

The easiest and fastest would be to apply a concrete repair dressing like Ardex CD. This patch will stand up to vehicle traffic, is easy to mix and place and very fast drying.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
is it possible to replace just two squares of a patio? - lean - 10-11-2012, 11:49 AM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 10-13-2012, 08:39 PM
RE: is it possible to replace just two squares of a patio? - ILLENTINC - 11-15-2012, 02:24 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-15-2012, 02:30 PM
RE: is it possible to replace just two squares of a patio? - ILLENTINC - 11-15-2012, 02:38 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-15-2012, 02:40 PM
RE: is it possible to replace just two squares of a patio? - eaadams - 11-19-2012, 11:26 AM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-19-2012, 09:06 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 06:54 AM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-20-2012, 02:11 PM
RE: is it possible to replace just two squares of a patio? - CCR - 11-20-2012, 02:57 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 03:02 PM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-20-2012, 03:10 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 03:40 PM
RE: is it possible to replace just two squares of a patio? - CCR - 11-20-2012, 03:46 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-20-2012, 05:26 PM
RE: is it possible to replace just two squares of a patio? - Rubensgt40 - 11-21-2012, 07:54 PM
RE: is it possible to replace just two squares of a patio? - CC Solutions - 11-21-2012, 08:16 PM

Users browsing this thread:
1 Guest(s)