The warehouse investigation is very interesting, and it points out that each concrete slab is unique. There is no chart anyone can follow to tell when a slab will be dry, how hard it will get, where it will crack..... Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
curing compound - marks - 03-22-2011, 01:34 PM
RE: curing compound - eaadams - 03-22-2011, 02:01 PM
RE: curing compound - Ernesto - 03-22-2011, 03:34 PM
RE: curing compound - CC Solutions - 03-22-2011, 04:11 PM
RE: curing compound - eaadams - 03-22-2011, 05:34 PM
RE: curing compound - Ernesto - 03-22-2011, 07:35 PM
RE: curing compound - CC Solutions - 03-23-2011, 06:04 AM
RE: curing compound - eaadams - 03-23-2011, 09:25 AM
RE: curing compound - CC Solutions - 03-23-2011, 10:00 AM
RE: curing compound - eaadams - 03-24-2011, 09:30 PM
RE: curing compound - jnasvik - 03-25-2011, 05:04 AM
RE: curing compound - eaadams - 03-25-2011, 08:28 PM
RE: curing compound - CC Solutions - 04-01-2011, 07:58 AM

Users browsing this thread:
1 Guest(s)