I am thinking using the RapidRH system but cannot find how many tests should be used for 1000 sqft

08-24-2009, 07:36 AM #2
jf222 Unregistered
 
According to the ASTM standard, it's 3 tests for the first 1000 ft^2 and 1 test for each 1000 ft^2 after that.