Ouch.

I know. We missed a small hole. It was drilled for a rod from below, and we didn't see it under the floor patch. When the blaster went over it exposed it, and being a small 1/4" hole we just plain missed it!

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Well this may not exactly fit this forum... - CC Solutions - 07-24-2010, 09:07 PM
RE: Well this may not exactly fit this forum... - Ernesto - 08-22-2010, 08:36 AM
RE: Well this may not exactly fit this forum... - eaadams - 08-22-2010, 02:46 PM
RE: Well this may not exactly fit this forum... - CC Solutions - 09-20-2010, 02:09 PM
RE: Well this may not exactly fit this forum... - eaadams - 09-20-2010, 02:21 PM
RE: Well this may not exactly fit this forum... - CC Solutions - 09-20-2010, 03:08 PM

Users browsing this thread:
1 Guest(s)