Today I was mitigating a concrete slab on second floor and while we were putting down the epoxy someone walked in and said, "We have something dripping onto us in the lower level ER."

It seems that we found a crack that went all the way through a cast in place deck and the epoxy dripped right on a doctor as he was conducting an x-ray.

I've heard the doc is pretty P.O.'d.

Oops.... :O

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Well this may not exactly fit this forum... - CC Solutions - 07-24-2010, 09:07 PM
RE: Well this may not exactly fit this forum... - Ernesto - 08-22-2010, 08:36 AM
RE: Well this may not exactly fit this forum... - eaadams - 08-22-2010, 02:46 PM
RE: Well this may not exactly fit this forum... - CC Solutions - 09-20-2010, 02:09 PM
RE: Well this may not exactly fit this forum... - eaadams - 09-20-2010, 02:21 PM
RE: Well this may not exactly fit this forum... - CC Solutions - 09-20-2010, 03:08 PM

Users browsing this thread:
1 Guest(s)