Not likely. The weld keeps the floor sealed, not hold it together. It's most likely acclimation or product failure. I've seen jobs where the substrate shrunk and caused this also. Concrete can shrink more than 1/4" every 20 feet....

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Vet Clinic - Ernesto - 12-04-2011, 09:58 AM
RE: Vet Clinic - CC Solutions - 12-05-2011, 06:33 PM
RE: Vet Clinic - eaadams - 12-05-2011, 06:37 PM
RE: Vet Clinic - Ernesto - 12-05-2011, 07:11 PM
RE: Vet Clinic - eaadams - 12-06-2011, 10:33 AM
RE: Vet Clinic - Ernesto - 12-06-2011, 10:42 AM
RE: Vet Clinic - eaadams - 12-06-2011, 01:38 PM
RE: Vet Clinic - Ernesto - 12-06-2011, 02:06 PM
RE: Vet Clinic - eaadams - 12-06-2011, 02:48 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 11:59 AM
RE: Vet Clinic - CC Solutions - 12-07-2011, 12:07 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 12:53 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 01:17 PM
RE: Vet Clinic - eaadams - 12-07-2011, 02:26 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 02:45 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 04:06 PM
RE: Vet Clinic - CC Solutions - 12-07-2011, 04:36 PM
RE: Vet Clinic - Ernesto - 12-07-2011, 07:58 PM
RE: Vet Clinic - CC Solutions - 12-08-2011, 12:02 AM
RE: Vet Clinic - eaadams - 12-23-2011, 12:15 PM
RE: Vet Clinic - Ernesto - 12-23-2011, 10:31 PM

Users browsing this thread:
1 Guest(s)