(10-13-2012, 08:35 PM)CC Solutions Wrote:  The RH of a slab can lead to increased vapor drive, as vapor drive is a function of differential vapor pressures. So a wet slab will release more vapor to dry air, and a dry slab will release less, or I should say release vapor at a slower rate.


I see so high RH = higher vapor but we don't have an accurate test for vapor so our best guess is RH as a predictor. Let's leave Osmosis out of the conversation for now. How do I measure vapor if the science behind the ASTM is no good?

I can see this question happening to me and want to have my answer ready for some day...








Messages In This Thread
Vapor Drive / Osmotic Action & RH - eaadams - 10-08-2012, 10:12 AM
RE: Vapor Drive / Osmotic Action & RH - CC Solutions - 10-13-2012, 08:35 PM
RE: Vapor Drive / Osmotic Action & RH - eaadams - 10-15-2012, 03:56 PM
RE: Vapor Drive / Osmotic Action & RH - CC Solutions - 10-15-2012, 04:18 PM
RE: Vapor Drive / Osmotic Action & RH - kayandrew - 12-15-2012, 04:22 AM
RE: Vapor Drive / Osmotic Action & RH - CC Solutions - 12-15-2012, 06:46 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
35 Replies 83,128 Views
Last Post by jim decker
05-01-2013, 07:20 AM
2 Replies 8,690 Views
Last Post by Ernesto
04-01-2012, 09:08 AM

Users browsing this thread:
1 Guest(s)