Bidding on some smaller commercial jobs now just cus it is slow in residential and he wants more money. I have not been doing commercial for quite awhile now so looking for feedback.
The building is old, vct is over cutback residue but stuck. We all know how iffy it is going over vct with new vct. I always write in a Rh test. Also stated if the reading is high the old vct gets demo'd as I've seen many a covered vct floor fail out here.
Product is Armstrong and they say you can go over one layer. Armstrong also highly reccommends an Rh test or meter or CaCl. Ha Ha Wondering if I should upcharge the install and throw in the Rh test free. These things are not cheap.
In my quote I always give links to the mans install requirements so they are somewhat educated . Hope I get this one as they are going to do three more buildings. Its a large moving rental company. hint hint.

Stephen Perrera dba
Top Floor Installation Co.

Messages In This Thread
VCT Over CutBack - Ernesto - 02-04-2014, 10:27 AM
RE: VCT Over CutBack - eaadams - 02-19-2014, 10:37 AM
RE: VCT Over CutBack - CC Solutions - 02-25-2014, 06:04 PM
RE: VCT Over CutBack - eaadams - 02-25-2014, 10:50 PM
RE: VCT Over CutBack - hausenheimer - 02-26-2014, 06:58 AM
RE: VCT Over CutBack - M.K.Pecou - 02-26-2014, 07:30 AM
RE: VCT Over CutBack - CC Solutions - 02-26-2014, 04:37 PM
RE: VCT Over CutBack - Ernesto - 02-27-2014, 03:02 PM

Users browsing this thread:
1 Guest(s)