I tried to post a comment but I couldn't... I hit 'submit' and it doesn't do anything... I was going to post:

I still have unanswered questions:

Is there a single flooring or adhesive manufacturer recognizing a slab tested by ASTM D-5084? And is each pour of a slab actually tested or is there one blanket test that covers all slabs poured?

Can a silicate treated slab (topical or integral) be tested using methods recognized by any major flooring or adhesive manufacturer?

I ask because when I test slabs treated integrally my MVER tests are higher than the same slab without the admix. And I cannot perform ASTM F-1869 on a topically treated slab without damaging the installation.

Therefore these treatment systems are unable to be proven in the field, and as far as I know, unaccepted by the flooring and adhesive manufacturers.

That leaves the owner and installer at great risk in the case of a failure.


I wrote to Bill to see if he could get my comment in.... Wink

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
The big donut - CC Solutions - 03-21-2013, 07:29 PM
RE: The big donut - CCR - 03-23-2013, 04:09 AM
RE: The big donut - CC Solutions - 03-25-2013, 05:55 AM
RE: The big donut - eaadams - 04-29-2013, 04:07 PM
RE: The big donut - CCR - 04-29-2013, 05:21 PM
RE: The big donut - eaadams - 04-29-2013, 05:26 PM
RE: The big donut - CCR - 04-29-2013, 05:48 PM
RE: The big donut - eaadams - 04-29-2013, 06:18 PM
RE: The big donut - CC Solutions - 04-29-2013, 06:48 PM
RE: The big donut - jim decker - 04-29-2013, 08:16 PM
RE: The big donut - CC Solutions - 04-29-2013, 08:38 PM

Users browsing this thread:
1 Guest(s)