04-29-2013, 05:48 PM #7
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
I was able to access the blog but unfortunately have to go back to read all the comments in sequence later.

That being said, my only comment (if I'm grasping this altogether right) is that it sounds like they're not shot blasting or grinding the failed product off before applying layer upon layer of different remediation product.Huh

If so, it's like painting over a bad paint job with a different paint hoping that the top coat holds...it ain't happenin! They're in for failure after failure after failure.....every layer is only as good as the bond of the product in direct contact with the concrete.

Either someone is not reading the directions, or sales people are telling them something like "it's just like Ardex, but you don't have to prep"

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
The big donut - CC Solutions - 03-21-2013, 07:29 PM
RE: The big donut - CCR - 03-23-2013, 04:09 AM
RE: The big donut - CC Solutions - 03-25-2013, 05:55 AM
RE: The big donut - eaadams - 04-29-2013, 04:07 PM
RE: The big donut - CCR - 04-29-2013, 05:21 PM
RE: The big donut - eaadams - 04-29-2013, 05:26 PM
RE: The big donut - CCR - 04-29-2013, 05:48 PM
RE: The big donut - eaadams - 04-29-2013, 06:18 PM
RE: The big donut - CC Solutions - 04-29-2013, 06:48 PM
RE: The big donut - jim decker - 04-29-2013, 08:16 PM
RE: The big donut - CC Solutions - 04-29-2013, 08:38 PM

Users browsing this thread:
2 Guest(s)