07-26-2012, 12:57 PM #18
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
All makes sense. Obvious testing challenge with garages and concrete roofs (a previous thread), is that service conditions have a huge swing. Today was about as hot and steamy as we get here. Come January, it could be 0 degrees. The particular manufacturer of the coating system specifies ASTM 1869 for testing, which makes no sense to me (except for that's what everyone did for years). However, they also recognize RH testing now and accept readings of 80%. It would be great to get input from Jason on this subject. It would make for a very good article in the online newsletter.

I think the best thing for me to do is include my standard disclaimer about readings being accurate at time of test and future results may vary, etc., etc.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
Testing Cost - eaadams - 06-06-2012, 07:25 PM
RE: Testing Cost - Ernesto - 06-07-2012, 05:59 PM
RE: Testing Cost - CCR - 06-10-2012, 04:21 AM
RE: Testing Cost - CC Solutions - 06-12-2012, 10:39 AM
RE: Testing Cost - CCR - 06-13-2012, 05:14 PM
RE: Testing Cost - CC Solutions - 06-13-2012, 06:46 PM
RE: Testing Cost - eaadams - 06-14-2012, 10:19 AM
RE: Testing Cost - CC Solutions - 06-14-2012, 10:45 AM
RE: Testing Cost - CCR - 06-14-2012, 05:49 PM
RE: Testing Cost - CC Solutions - 06-14-2012, 07:37 PM
RE: Testing Cost - CCR - 06-15-2012, 05:48 AM
RE: Testing Cost - CCR - 07-26-2012, 08:36 AM
RE: Testing Cost - CC Solutions - 07-26-2012, 08:49 AM
RE: Testing Cost - CCR - 07-26-2012, 08:53 AM
RE: Testing Cost - CC Solutions - 07-26-2012, 09:48 AM
RE: Testing Cost - CCR - 07-26-2012, 10:16 AM
RE: Testing Cost - CC Solutions - 07-26-2012, 10:54 AM
RE: Testing Cost - CCR - 07-26-2012, 12:57 PM
RE: Testing Cost - CC Solutions - 07-26-2012, 02:36 PM
RE: Testing Cost - rapidrhrep - 07-27-2012, 08:07 AM
RE: Testing Cost - CCR - 07-27-2012, 12:36 PM
RE: Testing Cost - CC Solutions - 07-30-2012, 04:39 PM
RE: Testing Cost - Ernesto - 07-30-2012, 07:01 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 7,295 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
2 Replies 7,416 Views
Last Post by eaadams
09-27-2013, 10:26 AM
33 Replies 64,921 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 110,682 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 11,987 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
36 Replies 84,378 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 25,783 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM
2 Replies 10,480 Views
Last Post by eaadams
09-30-2010, 08:27 AM
11 Replies 32,608 Views
Last Post by CC Solutions
09-20-2010, 03:01 PM
15 Replies 40,777 Views
Last Post by Ernesto
01-12-2010, 10:56 AM

Users browsing this thread:
1 Guest(s)