#Login Register
Test Before You Spec!
  • 0 Vote(s) - 0 Average


03-22-2013, 07:12 AM #3
jim decker Concrete Moisture Enthusiast *
Status: Offline Posts:42 Threads:4 Joined:Nov 2011
Yes it is and with wood it is even more noticeable though one only has to go through most floors in El Paso and see control cracks showing through saw on national chain grocery the other day looked like the floor had the mumps. Tested a Big Lots store removal revealed gypsum patch, emulsified adhesive really sad.








Messages In This Thread
Test Before You Spec! - CCR - 03-21-2013, 04:57 PM
RE: Test Before You Spec! - CC Solutions - 03-21-2013, 07:03 PM
RE: Test Before You Spec! - jim decker - 03-22-2013, 07:12 AM
RE: Test Before You Spec! - eaadams - 05-10-2013, 09:26 AM
RE: Test Before You Spec! - CC Solutions - 05-10-2013, 09:58 AM
RE: Test Before You Spec! - eaadams - 05-10-2013, 10:09 AM
RE: Test Before You Spec! - Ernesto - 05-13-2013, 04:51 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
10 Replies 22,983 Views
Last Post by eaadams
01-18-2013, 04:48 PM
16 Replies 39,332 Views
Last Post by CC Solutions
08-08-2011, 11:41 AM
3 Replies 13,775 Views
Last Post by Ernesto
08-30-2010, 12:42 PM
5 Replies 16,242 Views
Last Post by Ernesto
07-12-2010, 07:00 PM
2 Replies 10,378 Views
Last Post by eaadams
07-09-2010, 09:45 AM
14 Replies 42,752 Views
Last Post by CC Solutions
01-15-2010, 09:36 PM
2 Replies 10,959 Views
Last Post by CC Solutions
12-16-2009, 11:45 AM
3 Replies 14,269 Views
Last Post by rthompson
11-04-2008, 10:03 AM

Users browsing this thread:
1 Guest(s)