09-27-2013, 06:36 AM #2
FloorMaven Newbie *
Status: Offline Posts:1 Threads:0 Joined:Sep 2013
Personally I like to see product manufacturers take on a bit more of the liability when it comes to moisture issues...even if it means producing a product (as in this case?) has higher tolerances.

As far as being fair to owners, all's fair in love and business, or so I have heard. Personally, I hate sticker-shock and try to be realistic and upfront with my customers on what costs to expect. Consequently, I lose out on a lot of work (especially in the commercial arena) to the low initial bidders or those that tend not to manage customer's expectations.

But that is the nature of the beast...I'm sure many have seen the old photo of the two boats? The dingy named "Original Contract" and the yacht named "Change Order". That pretty much says it all.

.jpg 1-change-order.jpg Size: 72.45 KB  Downloads: 4

FloorMaven.com
Expert Floor Installation & Repair








Messages In This Thread
Tandus removes moisture testing requirement - eaadams - 09-13-2013, 09:07 AM
RE: Tandus removes moisture testing requirement - FloorMaven - 09-27-2013, 06:36 AM
RE: Tandus removes moisture testing requirement - eaadams - 09-27-2013, 10:26 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 6,330 Views
Last Post by Rubensgt40
07-05-2014, 03:18 AM
4 Replies 8,228 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 20,828 Views
Last Post by eaadams
05-19-2014, 10:55 AM
2 Replies 5,615 Views
Last Post by Rubensgt40
05-10-2014, 08:07 PM
33 Replies 69,408 Views
Last Post by eaadams
11-21-2012, 10:19 AM
51 Replies 118,261 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 12,806 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 47,444 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
23 Replies 65,807 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
5 Replies 15,095 Views
Last Post by Ernesto
08-14-2011, 08:43 PM

Users browsing this thread:
1 Guest(s)