Successful floor repair after failure!
  • 0 Vote(s) - 0 Average


09-28-2011, 02:20 PM #9
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
No difference except for getting paid and maybe working with unions...
Concrete is concrete, and drywall is drywall. You can tape plastic to the walls and seal the bottom edge to the floor and blast a hurricane in someone's basement if you'd like, and really there would be no difference than if you were in a commercial hallway.

What do you think the difference is? Huh

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Successful floor repair after failure! - CC Solutions - 09-23-2011, 06:27 AM
RE: Successful floor repair after failure! - Ernesto - 09-26-2011, 10:29 AM
RE: Successful floor repair after failure! - CC Solutions - 09-26-2011, 06:16 PM
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 06:33 AM
RE: Successful floor repair after failure! - CC Solutions - 09-27-2011, 06:39 AM
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 08:10 PM
RE: Successful floor repair after failure! - CC Solutions - 09-28-2011, 06:20 AM
RE: Successful floor repair after failure! - Ernesto - 09-28-2011, 06:44 AM
RE: Successful floor repair after failure! - CC Solutions - 09-28-2011, 02:20 PM
RE: Successful floor repair after failure! - Ernesto - 09-28-2011, 02:51 PM
RE: Successful floor repair after failure! - FloorMedic's - 09-28-2011, 08:42 PM
RE: Successful floor repair after failure! - CC Solutions - 09-29-2011, 05:07 AM
RE: Successful floor repair after failure! - Ernesto - 09-29-2011, 06:48 AM
RE: Successful floor repair after failure! - CC Solutions - 09-29-2011, 06:53 AM
RE: Successful floor repair after failure! - eaadams - 09-29-2011, 08:42 PM
RE: Successful floor repair after failure! - CC Solutions - 09-30-2011, 07:55 AM
RE: Successful floor repair after failure! - foxgeorge - 12-15-2011, 01:46 AM
RE: Successful floor repair after failure! - Adonis - 12-19-2011, 11:54 PM
RE: Successful floor repair after failure! - mableswift - 12-22-2011, 10:13 PM
RE: Successful floor repair after failure! - eaadams - 12-22-2011, 10:29 PM
RE: Successful floor repair after failure! - CC Solutions - 12-23-2011, 06:37 AM

Users browsing this thread:
1 Guest(s)