CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Or they do a bond test on an area they rinsed really well.

The adhesive dissolvers will turn the glue into a slurry that will absorb into the concrete. It's pretty darn hard to get all those chemicals out of the concrete. And once again, anything like that in the concrete voids the adhesive manufacturer's warranty.

I recommend mechanically removing all adhesives. Although I have made some good money coming in to mitigate after the chemical companies leave. Big Grin

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Successful floor repair after failure! - CC Solutions - 09-23-2011, 06:27 AM
RE: Successful floor repair after failure! - Ernesto - 09-26-2011, 10:29 AM
RE: Successful floor repair after failure! - CC Solutions - 09-26-2011, 06:16 PM
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 06:33 AM
RE: Successful floor repair after failure! - CC Solutions - 09-27-2011, 06:39 AM
RE: Successful floor repair after failure! - Ernesto - 09-27-2011, 08:10 PM
RE: Successful floor repair after failure! - CC Solutions - 09-28-2011, 06:20 AM
RE: Successful floor repair after failure! - Ernesto - 09-28-2011, 06:44 AM
RE: Successful floor repair after failure! - CC Solutions - 09-28-2011, 02:20 PM
RE: Successful floor repair after failure! - Ernesto - 09-28-2011, 02:51 PM
RE: Successful floor repair after failure! - FloorMedic's - 09-28-2011, 08:42 PM
RE: Successful floor repair after failure! - CC Solutions - 09-29-2011, 05:07 AM
RE: Successful floor repair after failure! - Ernesto - 09-29-2011, 06:48 AM
RE: Successful floor repair after failure! - CC Solutions - 09-29-2011, 06:53 AM
RE: Successful floor repair after failure! - eaadams - 09-29-2011, 08:42 PM
RE: Successful floor repair after failure! - CC Solutions - 09-30-2011, 07:55 AM
RE: Successful floor repair after failure! - foxgeorge - 12-15-2011, 01:46 AM
RE: Successful floor repair after failure! - Adonis - 12-19-2011, 11:54 PM
RE: Successful floor repair after failure! - mableswift - 12-22-2011, 10:13 PM
RE: Successful floor repair after failure! - eaadams - 12-22-2011, 10:29 PM
RE: Successful floor repair after failure! - CC Solutions - 12-23-2011, 06:37 AM

Users browsing this thread:
1 Guest(s)