If there is standing water under the slab, mitigating one part won't increase the amount of water under another part. That would be saying the portion you have mitigated was substantially drying the slab in one area and you have now plugged the leak in the dam. That just doesn't happen.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Substrate Odor - CCR - 05-19-2012, 06:06 AM
RE: Substrate Odor - CC Solutions - 05-20-2012, 09:15 AM
RE: Substrate Odor - CCR - 05-20-2012, 02:07 PM
RE: Substrate Odor - CC Solutions - 05-20-2012, 10:18 PM
RE: Substrate Odor - CCR - 05-21-2012, 03:34 AM
RE: Substrate Odor - CC Solutions - 05-21-2012, 06:45 AM
RE: Substrate Odor - Matt S - 05-22-2012, 06:19 PM
RE: Substrate Odor - CC Solutions - 05-22-2012, 07:07 PM
RE: Substrate Odor - Matt S - 05-22-2012, 07:16 PM
RE: Substrate Odor - CCR - 05-23-2012, 06:02 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 06:16 AM
RE: Substrate Odor - Matt S - 05-23-2012, 06:58 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 07:38 AM
RE: Substrate Odor - CCR - 05-23-2012, 07:46 AM
RE: Substrate Odor - Matt S - 05-23-2012, 09:51 AM
RE: Substrate Odor - eaadams - 05-24-2012, 12:58 PM
RE: Substrate Odor - CCR - 05-24-2012, 04:45 PM
RE: Substrate Odor - CC Solutions - 05-27-2012, 09:54 PM
RE: Substrate Odor - CCR - 06-15-2012, 11:02 AM
RE: Substrate Odor - CCR - 07-15-2012, 06:15 AM
RE: Substrate Odor - eaadams - 07-18-2012, 11:09 AM
RE: Substrate Odor - CCR - 07-18-2012, 11:36 AM

Users browsing this thread:
1 Guest(s)