#Login Register
Substrate Odor
  • 0 Vote(s) - 0 Average


05-23-2012, 06:02 AM #10
CCR Concrete Moisture Coach ***
Status: Offline Posts:236 Threads:14 Joined:Dec 2011
Compare MVE to a pot of boiling water... steam does not move sideways as it rises out of the pot. Same principal. Moisture vapor emissions move straight up, yet CAN migrate latteraly to some degree. Therefore, I was trained to add a foor or two to the perimeter of any MM system installation similar to mine.

Update: I provided an estimate yesterday to the customer covering the "conservative" fix, vs. installation of a MM system. For about $700 more, they get a warranted fix. I suspect they will go with the system and be done with this problem.

JK Nixon
Concrete Restoration Services, LLC
Pittsburgh, PA
http://www.rhtester.com








Messages In This Thread
Substrate Odor - CCR - 05-19-2012, 06:06 AM
RE: Substrate Odor - CC Solutions - 05-20-2012, 09:15 AM
RE: Substrate Odor - CCR - 05-20-2012, 02:07 PM
RE: Substrate Odor - CC Solutions - 05-20-2012, 10:18 PM
RE: Substrate Odor - CCR - 05-21-2012, 03:34 AM
RE: Substrate Odor - CC Solutions - 05-21-2012, 06:45 AM
RE: Substrate Odor - Matt S - 05-22-2012, 06:19 PM
RE: Substrate Odor - CC Solutions - 05-22-2012, 07:07 PM
RE: Substrate Odor - Matt S - 05-22-2012, 07:16 PM
RE: Substrate Odor - CCR - 05-23-2012, 06:02 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 06:16 AM
RE: Substrate Odor - Matt S - 05-23-2012, 06:58 AM
RE: Substrate Odor - CC Solutions - 05-23-2012, 07:38 AM
RE: Substrate Odor - CCR - 05-23-2012, 07:46 AM
RE: Substrate Odor - Matt S - 05-23-2012, 09:51 AM
RE: Substrate Odor - eaadams - 05-24-2012, 12:58 PM
RE: Substrate Odor - CCR - 05-24-2012, 04:45 PM
RE: Substrate Odor - CC Solutions - 05-27-2012, 09:54 PM
RE: Substrate Odor - CCR - 06-15-2012, 11:02 AM
RE: Substrate Odor - CCR - 07-15-2012, 06:15 AM
RE: Substrate Odor - eaadams - 07-18-2012, 11:09 AM
RE: Substrate Odor - CCR - 07-18-2012, 11:36 AM