09-17-2011, 02:07 PM #1
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Question If it is true that SCC has lower permeability than normal concrete, does this mean it dry's slower?
Question Thus resulting in less curling? Or are shrinkage reducing admixtures still greatly needed?

Certainly looks to me that SCC can't be used over a sand blotter layer... which seems like a very good thing for Div 9 people.

Question Is SCC to be tested differently for moisture?

Question Do moisture sealing companies treat SCC differently?

Question Any other things I should know?



Amazing stuff to see on YouTube about SCC.

I think concrete construction is doing an issue on it. That is the current poll on: http://www.concreteconstruction.net/








Messages In This Thread
Self consolidating concrete (SCC) - eaadams - 09-17-2011, 02:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-17-2011, 03:46 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-18-2011, 09:23 AM
RE: Self consolidating concrete (SCC) - rthompson - 09-28-2011, 05:37 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-28-2011, 08:14 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-29-2011, 08:29 AM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 05:48 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-29-2011, 07:42 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-29-2011, 08:23 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 09-30-2011, 08:15 AM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 12:30 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 04:02 PM
RE: Self consolidating concrete (SCC) - Ernesto - 09-30-2011, 05:36 PM
RE: Self consolidating concrete (SCC) - eaadams - 09-30-2011, 06:09 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-01-2011, 05:29 AM
RE: Self consolidating concrete (SCC) - Ernesto - 10-01-2011, 07:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-01-2011, 08:06 AM
RE: Self consolidating concrete (SCC) - eaadams - 10-01-2011, 08:39 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-02-2011, 12:07 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-02-2011, 05:07 PM
RE: Self consolidating concrete (SCC) - eaadams - 10-02-2011, 07:02 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 05:58 AM
RE: Self consolidating concrete (SCC) - rthompson - 10-03-2011, 07:31 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-03-2011, 08:32 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-07-2011, 06:09 AM
RE: Self consolidating concrete (SCC) - EWagner - 10-13-2011, 10:18 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 10-13-2011, 10:38 AM
RE: Self consolidating concrete (SCC) - foxgeorge - 12-15-2011, 12:59 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 12-15-2011, 11:41 AM
RE: Self consolidating concrete (SCC) - JDJR - 05-07-2012, 12:55 PM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-07-2012, 01:34 PM
RE: Self consolidating concrete (SCC) - JDJR - 05-08-2012, 04:24 AM
RE: Self consolidating concrete (SCC) - CC Solutions - 05-08-2012, 07:04 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 8,417 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 21,325 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 36,029 Views
Last Post by eaadams
11-08-2013, 01:41 PM
35 Replies 88,884 Views
Last Post by jim decker
05-01-2013, 07:20 AM
4 Replies 12,483 Views
Last Post by eaadams
01-30-2013, 04:43 PM
0 Replies 5,019 Views
Last Post by eaadams
03-23-2012, 09:40 AM
23 Replies 66,444 Views
Last Post by foxgeorge
12-15-2011, 01:20 AM
12 Replies 36,855 Views
Last Post by CC Solutions
06-21-2011, 11:47 AM
8 Replies 22,866 Views
Last Post by CC Solutions
06-09-2011, 06:09 AM

Users browsing this thread:
1 Guest(s)