08-31-2011, 02:59 PM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,067 Threads:69 Joined:Dec 2009
Dirt can be vacuumed or blown out of the sensor tube, usually with no problem.

Placing a cone over the test site is like placing a bullseye on something. They will hit it for sure!!! But seriously, anything that will disrupt or impede the drying of the slab will affect the RH in that area. So I would say placing a sealed 16" diameter rubber cone over the test site will hold vapor emissions and slow the slab's drying in that area. A small open top cone may effect drying a slight bit, but probably not enough to cause a noticeable difference.

I always try to put tests in locations that people aren't driving over the caps.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
Scissor Lift knocing off probe tops. - eaadams - 08-31-2011, 01:37 PM
RE: Scissor Lift knocing off probe tops. - CC Solutions - 08-31-2011, 02:59 PM
RE: Scissor Lift knocing off probe tops. - CC Solutions - 09-02-2011, 06:25 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post

Users browsing this thread:
1 Guest(s)