Anyone ever use a Schmidt hammer? How? Can they be used on 365+ day old concrete?

I'm considering investing in one but don't know how they work.

I'm starting to think a lot of my headaches are from either
a) soft crete - concrete that has a surface problem that falls apart after I have the floor down
b) hard crete - hard troweled concrete that inhibits a normal speed of moisture movement out of the slab.








Messages In This Thread
Schmidt hammer - eaadams - 10-26-2011, 09:46 PM
RE: Schmidt hammer - CC Solutions - 10-28-2011, 11:41 AM
RE: Schmidt hammer - eaadams - 11-02-2011, 10:24 PM
RE: Schmidt hammer - CC Solutions - 11-03-2011, 06:56 AM