10-03-2012, 07:45 PM #2
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:85 Threads:3 Joined:Aug 2011
EA: If I am seeing the question correctly, you want to know how to profile a floor, utilizing RH testing, correct? If this is the case, based on the science, people will typically install the sensors at varying depths in the floor, say at 1" depth variances. Of course this is done prior to flooring installation and this will allow you to see the moisture gradient in the slab.

Jason








Messages In This Thread
Reverse Curl & Relaxation - eaadams - 10-03-2012, 11:36 AM
RE: Reverse Curl & Relaxation - rapidrhrep - 10-03-2012, 07:45 PM
RE: Reverse Curl & Relaxation - eaadams - 10-04-2012, 10:21 AM
RE: Reverse Curl & Relaxation - CC Solutions - 10-07-2012, 07:11 PM
RE: Reverse Curl & Relaxation - eaadams - 10-02-2013, 12:58 PM