#Login Register
Relative Humidity Hysteresis
  • 0 Vote(s) - 0 Average


02-20-2014, 12:35 PM #5
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Have a slab that is sitting at 99% but some probes are dropping. It is new, closed off from elements all winter, no sand under slab. How do I know if the stuff hanging at 99% are subject to Hysteresis?








Messages In This Thread
Relative Humidity Hysteresis - eaadams - 05-24-2013, 09:53 AM
RE: Relative Humidity Hysteresis - CC Solutions - 05-27-2013, 10:32 AM
RE: Relative Humidity Hysteresis - eaadams - 05-28-2013, 10:35 AM
RE: Relative Humidity Hysteresis - rapidrhrep - 05-30-2013, 10:17 AM
RE: Relative Humidity Hysteresis - eaadams - 02-20-2014, 12:35 PM
RE: Relative Humidity Hysteresis - rapidrhrep - 02-20-2014, 12:40 PM
RE: Relative Humidity Hysteresis - eaadams - 02-20-2014, 12:41 PM