What is Hysteresis and why do we care?

05-27-2013, 10:32 AM #2
CC Solutions Concrete Moisture Evangelist *******
Status: Offline Posts:1,065 Threads:69 Joined:Dec 2009
hysteresis |ˌhistəˈrēsis| noun Physics
the phenomenon in which the value of a physical property lags behind changes in the effect causing it, as for instance when magnetic induction lags behind the magnetizing force.


Layman's terms: RH probes can lag behind the actual reading by a small amount as the concrete humidity changes. You'll have to ask Jason or Ed if hysteresis can cause a lag greater than the percentage of variation inherent in the probes.

If I am close to a target RH before a go / no-go decision is going to be made, I insert a couple fresh probes to get new readings to compare.

I think this is really important if the probes started out reading in the high 90's. The alkalinity is so high at that RH I don't see how the sensors resist damage if they are exposed to it for a long period of time.

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com

05-28-2013, 10:35 AM #3
eaadams Concrete Moisture Expert *****
Status: Offline Posts:597 Threads:86 Joined:Jul 2010
Jason or Ed can hysteresis can cause a lag greater than the percentage of variation inherent in the probes?

05-30-2013, 10:17 AM #4
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:83 Threads:3 Joined:Aug 2011
Yes, at very high and very low RH%. This would usually require extended exposure to this environment. The key word to remember here are lag and temporary. In high RH% environments, IF hysteresis is in play, the sensor may lag behind temporarily until the true RH% goes below say 90%. As CC stated, we recommend if you know the slab is going to be high (i.e poured 45 days ago) then do a sampling to begin with and then if there is a question, add more towards the end. Hysteresis is not an absolute.

Jason

02-20-2014, 12:35 PM #5
eaadams Concrete Moisture Expert *****
Status: Offline Posts:597 Threads:86 Joined:Jul 2010
Have a slab that is sitting at 99% but some probes are dropping. It is new, closed off from elements all winter, no sand under slab. How do I know if the stuff hanging at 99% are subject to Hysteresis?

02-20-2014, 12:40 PM #6
rapidrhrep Concrete Moisture Tutor **
Status: Offline Posts:83 Threads:3 Joined:Aug 2011
Mr Adams:

I hope all is well. The easiest way would be to put a couple of additional probes into the slab now to get some comparative data.

Jason

02-20-2014, 12:41 PM #7
eaadams Concrete Moisture Expert *****
Status: Offline Posts:597 Threads:86 Joined:Jul 2010
ok.

project is in Eureka... about as close as I get to you guys in Oregon. So if you get any calls... from SHN Engineers... you have context