Engineered wood ok to glue direct to concrete. Solid wood IF the boards are straight BUT generally one needs to use a screwdriver as a lever to get them tight together and then nail them. Dodgy

Also engineered wood can be blue taped to hold them in place until the glue sets while 3/4" solid..............Well just won't happen. Not to say it can't be done but success rate is diminished. Huh

Also most mfg don't advocate doing so and will wash their hands if it fails.Tongue