I attended a wood flooring job where a slab took moisture from a plumbing failure. There was poly sheeting on the slab, 12mm ply then 13mm overlay solid timber. The whole thing buckled like buggery. So there are definitely points which poly cannot withstand. As JD always advises- see what the warranty says!

The problem with socialism is that you soon run out of other people's money.
- Margaret Thatcher









Messages In This Thread
RH in Concrete for Wood Floor with Vapor Membrane - eaadams - 06-14-2012, 10:31 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 06-14-2012, 10:51 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - eaadams - 06-14-2012, 10:56 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 06-14-2012, 10:59 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - eaadams - 06-14-2012, 12:20 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CCR - 06-14-2012, 05:56 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 06-15-2012, 07:01 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Rubensgt40 - 06-18-2012, 04:55 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 06-18-2012, 05:55 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - eaadams - 06-19-2012, 11:49 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 06-19-2012, 01:38 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Ernesto - 06-20-2012, 08:00 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - eaadams - 06-25-2012, 02:02 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - simmonsviolet - 08-22-2012, 04:44 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 08-22-2012, 06:37 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Ernesto - 08-22-2012, 10:50 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Rubensgt40 - 08-23-2012, 04:17 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Ernesto - 08-23-2012, 07:25 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 08-24-2012, 05:58 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Ernesto - 08-24-2012, 12:21 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 03-17-2013, 07:40 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Rubensgt40 - 03-17-2013, 08:25 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 03-18-2013, 08:44 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 03-19-2013, 06:34 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 03-22-2013, 07:20 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 03-22-2013, 01:36 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 03-22-2013, 02:19 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Rubensgt40 - 03-25-2013, 05:20 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 03-25-2013, 05:44 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Rubensgt40 - 03-25-2013, 08:47 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 03-26-2013, 06:13 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - CC Solutions - 03-26-2013, 06:27 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - Ernesto - 03-30-2013, 11:33 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - eaadams - 04-29-2013, 03:58 PM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 04-30-2013, 08:02 AM
RE: RH in Concrete for Wood Floor with Vapor Membrane - jim decker - 05-01-2013, 07:20 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 8,197 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
13 Replies 20,739 Views
Last Post by eaadams
05-19-2014, 10:55 AM
9 Replies 35,673 Views
Last Post by eaadams
11-08-2013, 01:41 PM
21 Replies 65,240 Views
Last Post by CCR
07-19-2013, 05:14 PM
4 Replies 12,276 Views
Last Post by eaadams
01-30-2013, 04:43 PM
5 Replies 16,246 Views
Last Post by CC Solutions
12-15-2012, 06:46 AM
32 Replies 80,874 Views
Last Post by CC Solutions
05-08-2012, 07:04 AM
2 Replies 9,139 Views
Last Post by Ernesto
04-01-2012, 09:08 AM
0 Replies 4,950 Views
Last Post by eaadams
03-23-2012, 09:40 AM
2 Replies 11,432 Views
Last Post by eaadams
12-23-2011, 12:06 PM

Users browsing this thread:
1 Guest(s)