I agree the architect and the GC should have known from the get-go that the floor had to have good conditions to dry. Then when they burned the snot out of it they should have known for sure it wasn't going to dry unless it was opened up so it could breathe.

The truth is, I bet they are both shaking their head blaming the flooring installer for the problem....

And what is the first letter of the flooring manufacturer's name?

JD Grafton
Concrete Answers for Flooring Problems
JGrafton@ccsolves.com








Messages In This Thread
RH Testing Thick Slabs - CCR - 09-24-2012, 06:21 PM
RE: RH Testing Thick Slabs - eaadams - 09-25-2012, 09:25 AM
RE: RH Testing Thick Slabs - CCR - 09-25-2012, 10:03 AM
RE: RH Testing Thick Slabs - eaadams - 09-25-2012, 10:06 AM
RE: RH Testing Thick Slabs - CCR - 09-25-2012, 10:13 AM
RE: RH Testing Thick Slabs - Rubensgt40 - 10-09-2012, 07:07 PM
RE: RH Testing Thick Slabs - CCR - 10-10-2012, 02:10 PM
RE: RH Testing Thick Slabs - Ernesto - 10-10-2012, 04:24 PM
RE: RH Testing Thick Slabs - CCR - 10-10-2012, 04:58 PM
RE: RH Testing Thick Slabs - Ernesto - 10-10-2012, 07:24 PM
RE: RH Testing Thick Slabs - CC Solutions - 10-13-2012, 08:29 PM
RE: RH Testing Thick Slabs - Ernesto - 10-14-2012, 08:19 AM
RE: RH Testing Thick Slabs - CC Solutions - 10-14-2012, 09:55 AM
RE: RH Testing Thick Slabs - Ernesto - 10-14-2012, 07:46 PM
RE: RH Testing Thick Slabs - CC Solutions - 10-15-2012, 06:07 AM
RE: RH Testing Thick Slabs - CCR - 10-17-2012, 01:07 PM
RE: RH Testing Thick Slabs - Ernesto - 10-18-2012, 08:01 PM
RE: RH Testing Thick Slabs - CCR - 10-19-2012, 05:39 AM
RE: RH Testing Thick Slabs - Ernesto - 10-19-2012, 06:41 PM
RE: RH Testing Thick Slabs - Rubensgt40 - 10-23-2012, 06:16 PM
RE: RH Testing Thick Slabs - Ernesto - 10-24-2012, 07:44 AM
RE: RH Testing Thick Slabs - rapidrhrep - 10-24-2012, 08:08 AM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 03:18 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 03:28 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 03:43 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:21 PM
RE: RH Testing Thick Slabs - eaadams - 11-20-2012, 05:26 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:30 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 05:33 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:35 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 05:45 PM
RE: RH Testing Thick Slabs - CC Solutions - 11-20-2012, 05:49 PM
RE: RH Testing Thick Slabs - CCR - 11-20-2012, 05:54 PM
RE: RH Testing Thick Slabs - eaadams - 11-21-2012, 10:19 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
4 Replies 7,242 Views
Last Post by Ashok Kakade
05-20-2014, 12:00 PM
4 Replies 9,258 Views
Last Post by CC Solutions
12-20-2013, 10:23 PM
2 Replies 7,387 Views
Last Post by eaadams
09-27-2013, 10:26 AM
21 Replies 61,761 Views
Last Post by CCR
07-19-2013, 05:14 PM
51 Replies 110,428 Views
Last Post by ILLENTINC
11-19-2012, 11:59 AM
4 Replies 11,960 Views
Last Post by CC Solutions
09-18-2012, 06:11 PM
22 Replies 44,569 Views
Last Post by Ernesto
07-30-2012, 07:01 PM
62 Replies 114,225 Views
Last Post by CC Solutions
12-07-2011, 07:27 AM
36 Replies 84,258 Views
Last Post by CC Solutions
04-19-2011, 04:59 PM
9 Replies 25,749 Views
Last Post by CC Solutions
04-05-2011, 05:33 AM

Users browsing this thread:
1 Guest(s)