I had a GC tell me the other day that he once was working on a prison hospital that was to receive vinyl flooring. He said what they did (and apparently worked) was super heat with heaters all night, come in in the morning, vent the room out with fans, close it up, super heat all day, vent at end of day, and repeat. Claims they dropped their moisture enough to get floor covering in a few weeks.

Sounds a lot like this Munters / Best Buy story ... I'd love to know how much such a system / process costs: http://www.munters.us/upload/Case%20studies/Best%20Buy%20Case%20Study.pdf








Messages In This Thread
RH Numbers Rising - COD - 04-05-2011, 09:40 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 10:49 AM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 11:49 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 12:19 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 12:27 PM
RE: RH Numbers Rising - COD - 04-05-2011, 01:16 PM
RE: RH Numbers Rising - CC Solutions - 04-05-2011, 05:26 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 08:42 PM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 06:04 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 07:40 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 08:23 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 08:28 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 04:54 PM
RE: RH Numbers Rising - CC Solutions - 04-07-2011, 06:12 AM
RE: RH Numbers Rising - rthompson - 04-07-2011, 01:08 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 08:01 AM
RE: RH Numbers Rising - CC Solutions - 04-08-2011, 08:06 AM
RE: RH Numbers Rising - rthompson - 04-08-2011, 10:33 AM
RE: RH Numbers Rising - eaadams - 04-08-2011, 04:19 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 04:54 PM
RE: RH Numbers Rising - eaadams - 04-08-2011, 05:00 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 08:59 AM
RE: RH Numbers Rising - rthompson - 04-09-2011, 11:57 AM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:14 PM
RE: RH Numbers Rising - eaadams - 04-09-2011, 01:38 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:46 PM
RE: RH Numbers Rising - rthompson - 04-09-2011, 02:06 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 02:39 PM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 09:49 AM
RE: RH Numbers Rising - CC Solutions - 04-11-2011, 09:54 AM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 08:50 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 12:26 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:10 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 01:20 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:28 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 03:08 PM
RE: RH Numbers Rising - eaadams - 04-18-2011, 04:46 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 04:55 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 05:15 PM
RE: RH Numbers Rising - Ernesto - 04-20-2011, 07:58 AM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 08:02 AM
RE: RH Numbers Rising - rthompson - 04-20-2011, 05:15 PM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 09:00 PM
RE: RH Numbers Rising - Ernesto - 04-23-2011, 07:01 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 07:59 PM
RE: RH Numbers Rising - CC Solutions - 04-23-2011, 08:59 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 10:01 PM
RE: RH Numbers Rising - Ernesto - 04-24-2011, 08:24 AM
RE: RH Numbers Rising - eaadams - 09-08-2011, 06:08 PM
RE: RH Numbers Rising - CC Solutions - 09-09-2011, 08:11 AM
RE: RH Numbers Rising - rthompson - 09-09-2011, 09:36 AM
RE: RH Numbers Rising - Ernesto - 09-09-2011, 04:48 PM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 09-10-2011, 11:14 AM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 06:30 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:22 AM
RE: RH Numbers Rising - rthompson - 09-11-2011, 08:25 AM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:40 AM
RE: RH Numbers Rising - CC Solutions - 09-11-2011, 03:54 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 06:50 PM
RE: RH Numbers Rising - rthompson - 09-12-2011, 08:56 AM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 09:07 AM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 05:14 PM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 05:33 PM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 07:27 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:49 AM
RE: RH Numbers Rising - rthompson - 09-13-2011, 08:37 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 08:43 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 10:08 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 11:28 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 01:37 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 01:55 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:14 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 02:17 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:18 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 02:33 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 05:26 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:46 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:56 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 06:03 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 06:06 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:23 PM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 06:29 AM
RE: RH Numbers Rising - CC Solutions - 09-14-2011, 06:54 AM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 07:39 PM
RE: RH Numbers Rising - CC Solutions - 09-15-2011, 04:59 AM
RE: RH Numbers Rising - Ernesto - 09-20-2011, 08:07 PM
RE: RH Numbers Rising - CC Solutions - 09-20-2011, 08:30 PM
RE: RH Numbers Rising - Ernesto - 09-21-2011, 08:19 PM
RE: RH Numbers Rising - CC Solutions - 09-21-2011, 09:18 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:39 AM
RE: RH Numbers Rising - CC Solutions - 09-22-2011, 09:28 AM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 07:14 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 07:50 PM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 08:00 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:48 PM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 05:54 AM
RE: RH Numbers Rising - Ernesto - 09-23-2011, 06:58 AM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 10:37 AM

Users browsing this thread:
1 Guest(s)