I recently entered the 21st Century and started using the RH test in lieu of the Calcium Chloride tests. I have a new addition project where the slab is about 3 months old. The HVAC is not on yet, there is temporary heat in the building and the temperature is in the mid to low 60s. There is a moisture barrier under the slab.
I installed 4 probes at various locations in the slab, waited about 90 minutes and checked the results. The readings were between 91% and 94%. When I went back a week later all the readings had risen to 99%. Is this unusual?








Messages In This Thread
RH Numbers Rising - COD - 04-05-2011, 09:40 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 10:49 AM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 11:49 AM
RE: RH Numbers Rising - eaadams - 04-05-2011, 12:19 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 12:27 PM
RE: RH Numbers Rising - COD - 04-05-2011, 01:16 PM
RE: RH Numbers Rising - CC Solutions - 04-05-2011, 05:26 PM
RE: RH Numbers Rising - Ernesto - 04-05-2011, 08:42 PM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 06:04 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 07:40 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 08:23 AM
RE: RH Numbers Rising - CC Solutions - 04-06-2011, 08:28 AM
RE: RH Numbers Rising - Ernesto - 04-06-2011, 04:54 PM
RE: RH Numbers Rising - CC Solutions - 04-07-2011, 06:12 AM
RE: RH Numbers Rising - rthompson - 04-07-2011, 01:08 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 08:01 AM
RE: RH Numbers Rising - CC Solutions - 04-08-2011, 08:06 AM
RE: RH Numbers Rising - rthompson - 04-08-2011, 10:33 AM
RE: RH Numbers Rising - eaadams - 04-08-2011, 04:19 PM
RE: RH Numbers Rising - Ernesto - 04-08-2011, 04:54 PM
RE: RH Numbers Rising - eaadams - 04-08-2011, 05:00 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 08:59 AM
RE: RH Numbers Rising - rthompson - 04-09-2011, 11:57 AM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:14 PM
RE: RH Numbers Rising - eaadams - 04-09-2011, 01:38 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 01:46 PM
RE: RH Numbers Rising - rthompson - 04-09-2011, 02:06 PM
RE: RH Numbers Rising - CC Solutions - 04-09-2011, 02:39 PM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 09:49 AM
RE: RH Numbers Rising - CC Solutions - 04-11-2011, 09:54 AM
RE: RH Numbers Rising - Ernesto - 04-11-2011, 08:50 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 12:26 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:10 PM
RE: RH Numbers Rising - T_Schneider - 04-18-2011, 01:20 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 01:28 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 03:08 PM
RE: RH Numbers Rising - eaadams - 04-18-2011, 04:46 PM
RE: RH Numbers Rising - Ernesto - 04-18-2011, 04:55 PM
RE: RH Numbers Rising - CC Solutions - 04-18-2011, 05:15 PM
RE: RH Numbers Rising - Ernesto - 04-20-2011, 07:58 AM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 08:02 AM
RE: RH Numbers Rising - rthompson - 04-20-2011, 05:15 PM
RE: RH Numbers Rising - CC Solutions - 04-20-2011, 09:00 PM
RE: RH Numbers Rising - Ernesto - 04-23-2011, 07:01 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 07:59 PM
RE: RH Numbers Rising - CC Solutions - 04-23-2011, 08:59 PM
RE: RH Numbers Rising - rthompson - 04-23-2011, 10:01 PM
RE: RH Numbers Rising - Ernesto - 04-24-2011, 08:24 AM
RE: RH Numbers Rising - eaadams - 09-08-2011, 06:08 PM
RE: RH Numbers Rising - CC Solutions - 09-09-2011, 08:11 AM
RE: RH Numbers Rising - rthompson - 09-09-2011, 09:36 AM
RE: RH Numbers Rising - Ernesto - 09-09-2011, 04:48 PM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 07:47 AM
RE: RH Numbers Rising - Ernesto - 09-10-2011, 11:14 AM
RE: RH Numbers Rising - CC Solutions - 09-10-2011, 06:30 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:22 AM
RE: RH Numbers Rising - rthompson - 09-11-2011, 08:25 AM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 08:40 AM
RE: RH Numbers Rising - CC Solutions - 09-11-2011, 03:54 PM
RE: RH Numbers Rising - Ernesto - 09-11-2011, 06:50 PM
RE: RH Numbers Rising - rthompson - 09-12-2011, 08:56 AM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 09:07 AM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 05:14 PM
RE: RH Numbers Rising - CC Solutions - 09-12-2011, 05:33 PM
RE: RH Numbers Rising - Ernesto - 09-12-2011, 07:27 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:49 AM
RE: RH Numbers Rising - rthompson - 09-13-2011, 08:37 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 08:43 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 10:08 AM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 11:28 AM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 01:37 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 01:55 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:14 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 02:17 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 02:18 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 02:33 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 05:26 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:46 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 05:52 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 05:56 PM
RE: RH Numbers Rising - CC Solutions - 09-13-2011, 06:03 PM
RE: RH Numbers Rising - eaadams - 09-13-2011, 06:06 PM
RE: RH Numbers Rising - Ernesto - 09-13-2011, 07:23 PM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 06:29 AM
RE: RH Numbers Rising - CC Solutions - 09-14-2011, 06:54 AM
RE: RH Numbers Rising - Ernesto - 09-14-2011, 07:39 PM
RE: RH Numbers Rising - CC Solutions - 09-15-2011, 04:59 AM
RE: RH Numbers Rising - Ernesto - 09-20-2011, 08:07 PM
RE: RH Numbers Rising - CC Solutions - 09-20-2011, 08:30 PM
RE: RH Numbers Rising - Ernesto - 09-21-2011, 08:19 PM
RE: RH Numbers Rising - CC Solutions - 09-21-2011, 09:18 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:39 AM
RE: RH Numbers Rising - CC Solutions - 09-22-2011, 09:28 AM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 07:14 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 07:50 PM
RE: RH Numbers Rising - Ernesto - 09-22-2011, 08:00 PM
RE: RH Numbers Rising - eaadams - 09-22-2011, 08:48 PM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 05:54 AM
RE: RH Numbers Rising - Ernesto - 09-23-2011, 06:58 AM
RE: RH Numbers Rising - CC Solutions - 09-23-2011, 10:37 AM

Users browsing this thread:
1 Guest(s)