07-12-2012, 01:31 PM #4
eaadams Concrete Moisture Expert *****
Status: Offline Posts:600 Threads:88 Joined:Jul 2010
Yea we don't accept CaCl tests anymore. Even people with a P.E. after their name seem to not be able to do it correctly. These pictures done by one of the more respected "professional building testing labs" in California.

Here is an example of this.
[Image: IMG_1475.JPG]




side note: oy the cracks Sad Lumpy Bumpy Slab will probably break poor church's budget. We want to fix the crack with Roadware Concrete Mender but at over $5 lft it is so expensive.

[Image: IMG_1477.JPG]








Messages In This Thread
RH & CC Testing - CCR - 07-10-2012, 10:35 AM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 06:37 AM
RE: RH & CC Testing - CCR - 07-12-2012, 07:25 AM
RE: RH & CC Testing - eaadams - 07-12-2012, 01:31 PM
RE: RH & CC Testing - CCR - 07-12-2012, 01:38 PM
RE: RH & CC Testing - CC Solutions - 07-12-2012, 01:48 PM
RE: RH & CC Testing - JLG - 07-17-2012, 11:13 AM
RE: RH & CC Testing - CCR - 07-17-2012, 11:37 AM
RE: RH & CC Testing - Erica - 07-17-2012, 12:10 PM
RE: RH & CC Testing - CCR - 07-17-2012, 12:27 PM
RE: RH & CC Testing - eaadams - 07-18-2012, 11:19 AM
RE: RH & CC Testing - CCR - 07-18-2012, 11:32 AM
RE: RH & CC Testing - CC Solutions - 07-19-2012, 07:49 PM
RE: RH & CC Testing - CCR - 07-22-2012, 04:55 AM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 09:09 AM
RE: RH & CC Testing - CCR - 07-22-2012, 03:05 PM
RE: RH & CC Testing - Rubensgt40 - 07-22-2012, 07:19 PM
RE: RH & CC Testing - CC Solutions - 07-22-2012, 07:33 PM
RE: RH & CC Testing - CCR - 07-24-2012, 04:07 PM
RE: RH & CC Testing - Rubensgt40 - 07-24-2012, 05:35 PM
RE: RH & CC Testing - CC Solutions - 07-24-2012, 05:49 PM
RE: RH & CC Testing - CCR - 07-25-2012, 03:49 AM
RE: RH & CC Testing - Rubensgt40 - 07-25-2012, 09:46 PM
RE: RH & CC Testing - CC Solutions - 07-26-2012, 06:19 AM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
3 Replies 5,967 Views
Last Post by jim decker
07-13-2015, 02:51 PM
3 Replies 10,451 Views
Last Post by CC Solutions
09-01-2013, 09:10 AM
3 Replies 9,409 Views
Last Post by eaadams
06-28-2013, 10:26 AM
27 Replies 46,289 Views
Last Post by jim decker
05-02-2013, 12:31 PM
23 Replies 38,369 Views
Last Post by CCR
03-21-2013, 05:05 PM
6 Replies 14,865 Views
Last Post by CCR
07-12-2012, 01:44 PM
1 Replies 7,600 Views
Last Post by hnelson
06-07-2012, 01:08 PM

Users browsing this thread:
1 Guest(s)