#Login Register
Light Weight Concrete on Pan Deck
  • 0 Vote(s) - 0 Average


03-01-2012, 01:05 PM #3
arlington Newbie *
Status: Offline Posts:3 Threads:1 Joined:Mar 2012
Thanks for the feedback. We are using a Wagner model with separate probes. Given that the slab is 3". Are we correct in that the depth of the hole for the probe should be appx 1-1/6" deep? We were reading and came across a post that said the hole is to be 40% the slab depth. The holes that were used for the previous test are over 2" deep.








Messages In This Thread
Light Weight Concrete on Pan Deck - arlington - 03-01-2012, 12:05 PM
RE: Light Weight Concrete on Pan Deck - CC Solutions - 03-01-2012, 12:57 PM
RE: Light Weight Concrete on Pan Deck - arlington - 03-01-2012, 01:05 PM
RE: Light Weight Concrete on Pan Deck - CC Solutions - 03-01-2012, 01:18 PM
RE: Light Weight Concrete on Pan Deck - arlington - 03-27-2012, 10:43 AM
RE: Light Weight Concrete on Pan Deck - eaadams - 03-27-2012, 01:00 PM
RE: Light Weight Concrete on Pan Deck - CC Solutions - 03-27-2012, 01:08 PM

Possibly Related Threads...
Thread / Author Replies / Views Last Post
25 Replies 42,814 Views
Last Post by CC Solutions
02-26-2014, 03:20 PM
9 Replies 22,827 Views
Last Post by CC Solutions
12-26-2012, 01:02 PM

Users browsing this thread:
1 Guest(s)