Nope it is an indoor gym slab. Why would it have air is beyond my expertise (thus why I'm posting)

I'm not sure how you know what the cement % is. I have the Weight (lb) / Volume numbers for each part. Should I post that?

I also have a column called "specific gravity" but I don't think that is relevant.








Messages In This Thread
Kapow! Low RH by Sundt - eaadams - 05-06-2013, 09:42 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:31 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 06:39 PM
RE: Kapow! Low RH by Sundt - jim decker - 05-07-2013, 06:54 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 07:24 PM
RE: Kapow! Low RH by Sundt - Rubensgt40 - 05-07-2013, 08:38 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-07-2013, 08:40 PM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 09:36 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:14 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-10-2013, 10:22 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-10-2013, 10:26 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 09:41 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 09:48 AM
RE: Kapow! Low RH by Sundt - rapidrhrep - 05-24-2013, 10:09 AM
RE: Kapow! Low RH by Sundt - eaadams - 05-24-2013, 10:16 AM
RE: Kapow! Low RH by Sundt - CC Solutions - 05-27-2013, 10:17 AM

Users browsing this thread:
1 Guest(s)